Saltar al contenido principal

Welding the Inconel 718 Superalloy

Reduction of Micro-segregation and Laves Phases

  • 1 Edición - 29 de mayo de 2019
  • Última edición
  • Autores: S.G.K. Manikandan, D. Sivakumar, M. Kamaraj
  • Idioma: Inglés

Welding the Inconel 718 Superalloy: Reduction of Micro-segregation and Laves Phases explores the day-to-day welding business in Alloy 718 and presents solutions to avoid or minimi… Leer más

Descripción

Welding the Inconel 718 Superalloy: Reduction of Micro-segregation and Laves Phases explores the day-to-day welding business in Alloy 718 and presents solutions to avoid or minimize micro-segregation. It considers the limitations of changing from lab scale models to actual production models and presents new technologies with proven experimental background. Various case studies are presented within the text, as well as proposed solutions backed by experimental evidence. Items previewed in this edition include enhanced cooling rates in the GTA welding process with cryogenic cooling and enhanced dendrite refinement using modified pulse waveform.

This work will be useful to researchers from the aerospace, space, power generation, nuclear, and chemical industries, as well as students interested in superalloys and welding.

Puntos claves

  • Resolves the industrial limitations in reducing the formation of laves phases in the welding of alloy 718
  • Presents case studies in industrial applications
  • Discusses new technologies with proven experimental background
  • Includes a comparison of laves size and distribution between GTAW, EBW, LBW and FW

De interès para

Materials Scientists and researchers within the aerospace, power generation, and chemical industries; graduate students in the area of materials science and engineering

Índice

Chapter 1 IntroductionChapter 2 Physical metallurgy of alloy 7182.1 Alloy 7182.2 Welding and weldability of Alloy 718 Chapter 3 Objectives and scopeChapter 4 Experimental methods4.1 Details of base material4.2 Details of filler metal4.3 Solidification experiments4.4 Process parameters and pulse waveform4.5 Welding experiments4.6 Characterization methods4.7 Heat treatment4.8 Mechanical property evaluationChapter 5 Results and discussion5.1 Base material microstructures and mechanical properties5.2 Effect of modified pulse waveform on weld microstructure and mechanical properties5.3 Effect of liquid nitrogen cooling and modified pulse waveform on weld microstructure and mechanical properties5.4 Effect of high frequency superimposed over low pulse frequency on weld microstructure and mechanical propertiesChapter 6 Conclusion Appendix Scope for future work References

Detalles del producto

  • Edición: 1
  • Última edición
  • Publicado: 29 de mayo de 2019
  • Idioma: Inglés

Sobre los autores

S.G.K. Manikandan

Author
Dr.SGK.Manikandan is currently a Head of welding and coating facilities at ISRO propulsion complex, Indian Space Research Organisation, Mahendragiri. He graduated from Bharathiar University in 1997 and subsequently completed PhD at IIT Madras. He has more than 20 years of research and industrial experience in welding of stainless steels, aluminum alloys, titanium alloys and Superalloys. He has done extensive research on the physical metallurgy and welding of Superalloys. He has also developed welding processes and procedures for the requirement of Indian Space Programme. He has published and presented 20 research publications and guided 6 scholars for Masters Degree and PhD. He is the life member of Indian Institute of Metals, Indian Welding Society and Aeronautical Society of India. He is awarded with team performance excellence award of ISRO and Society of Aerospace Manufacturing Engineers.
Afiliaciones y experiencia
Head of Welding and Coating Facilities, ISRO Propulsion Complex, Indian Space Research Organisation, India

D. Sivakumar

Author
Dr.D.Sivakumar is currently a senior Scientist in the Materials & Metallurgy Group at Vikram Sarabhai Space Centre, Trivandrum, India. He graduated from IIT Madras in Metallurgy in 1986 and subsequently completed Ph.D at IIT Mumbai. He has more than 25 years of research and industrial experience in welding and brazing of stainless steels and superalloys. He has also done research on physical metallurgy and welding of maraging steels. He has published and presented more than 50 research publications and guided 5 Ph.D scholars.
Afiliaciones y experiencia
Senior Scientist, Vikiram Sarabhai Space Centre, India

M. Kamaraj

Author
Prof. Dr. M. Kamaraj is currently Professor in the Department of Metallurgical and Materials Engineering at Indian Institute of Technology Madras, Chennai, India. After completing his Ph.D. at I.I.T. Madras, he worked as Research Engineer at EWAC Alloys Ltd (Larsen & Toubro Ltd., ) Mumbai. He was also a Research Fellow at Nagaoka University of Technology and STA Fellow at the National Institute of Industrial Safety, Japan. He was a Guest Scientist at Ruhr-Universitat Bochum, Bochum, Germany and a visiting scientist at VSSC, Trivandrum, India. He joined I.I.T Madras, and has more than 25 years teaching, research and industrial experience in the area of mechanical behaviour of materials, welding, surface engineering, and high temperature behavior of materials/welded joints, Tribological behavior of composites and failure analysis of industrial components. He has a patent approval ( Invention: IN-813918), titled “ Highly adhesive nano crystalline diamond coatings on tin coated WC-Co( D/TiN/ Al2O3/ TiCN/WC) tools for industrial applications” He has guided 16 Ph.D and 4 MS scholars and Ph.D thesis examiner for several Institutes and Universities. He has published more than 150 research publication in leading national and international engineering journals. He has published books on Surface Modified Biomedical Titanium Alloys (ISBN: 978-1-60876-581-2 (2010) with Mr. Aravind Vadiraj and Surface Technology with V.M. Radhakrishnan (ISBN: 978-81-224-3960-1) and contributed a chapter on “Microstructure and Wear Studies of Alloyed and Austempered Gray Irons for Automotive Applications” along with Aravind Vadiraj and G. Balachandran. He was the chairman, Indian Institute of Metals, Chennai Chapter (2009-2010), Chairman, Indian welding Society Chennai centre (2008-2010), Member of ASM international, Chennai chapter (since 2001), and Life member of ISNT, Chennai centre.
Afiliaciones y experiencia
Professor, Dept of Metallurgical and Materials Engineering, Indian Institute of Technology Madras, India

Ver libro en ScienceDirect

Lee Welding the Inconel 718 Superalloy en ScienceDirect